A-A-584B
Table I
Visual examination
Examine |
Defects |
Color |
Not dark brown, not uniform. |
Shells |
Not reinforced vinyl Cracked, crazing, bubbles, or wrinkles. |
Interior |
Sharp, jagged, rough or unfinished components. Interior bubbled or wrinkled. Interior showing raw or unfinished edges. |
Hardware |
Misaligned, rough, unfinished, not plated when required, plating not uniform. |
Bumpers |
Do not support the case evenly on a level surface. |
Hinges |
Not covered by case material or made from leather of the same color as case material. |
Opening flaps |
Not supported adequately by hinges, i.e. sags. |
Rivets |
Not securely clinched. Raw or sharp edges points. |
Lock(s) |
Does not latch. None or not enough keys provided. Does not lock and unlock as required. |
Latches |
Do not mate at closing. Do not secure the case closed. |
Marking |
Omitted, incomplete, incorrect, illegible, wrong place. |
Workmanship. |
Any part fractured, ripped, torn, punctured, malformed, or otherwise damaged. |
Test conditions. Unless otherwise specified test apparatus may be of any design suitable for performing the test. All tests shall be conducted at 68 to 75 degrees Fahrenheit and 48 to 52 percent relative humidity, except that the cases for the drop test shall be loaded and conditioned at minus 10 + 5 degrees Fahrenheit, for a minimum of 4 hours in a refrigerated cabinet or chamber and then be tested immediately after removal from the cabinet.